When copper pyrite is roasted in excess of air, a mixture of Cu2S and FeO are formed. FeO is present as impurity. This can be removed as slag during Smelting. The flux added to form slag is
Options:
A .  Silica which is an acidic flux
B .  Limestone, which is a basic flux
C .  SiO2 which is a basic flux
D .  CaO which is a basic flux
Answer: Option A
:
A
FeO (Basic gangue) impurity is mixed with SiO2 (acidic flux) to form a fusible slag
FeO +SiO2 FeSiO3