The temperature required for full annealing in hyper-eutectoid steel is
Options:
A .  50°C above upper critical temperature
B .  50°C below upper critical temperature
C .  50°C above lower critical temperature
D .  50°C below lower critical temperature
Answer: Option C
Answer: (c).50°C above lower critical temperature